NIMONIC263/UNS N07263/2.4650
Alloy C263 (Nimonic C263) is a precipitation hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. Alloy C263 has high strength and corrosion resistance as well as having good formability and high temperature ductility in welded structures. Alloy C263 is used in gas turbines for rings, casings and various sheet fabrications.
Typical Mechanical Properties Typical Heat Treatments
Bar - Solution Treated for 2 hrs @ 1150°C + Water Quench - Age 8 hrs @ 800°C + Air Cool, Cold Rolled Sheet Solution Treated 3-10 mins @ 1150°C + Water Quench - Age 8 hrs @ 800°C + Air Cool