AL-6XN/UNS08367 AL-6XN alloy (UNS N08367) is a low carbon, high purity, nitrogen-bearing "super-austenitic" stainless alloy. The AL6XN alloy was designed to be a seawater resistant material and has since been demonstrated to be resistant to a broad range of very corrosive environments. The high strength and corrosion resistance of the AL6XN alloy make it a better choice than the conventional duplex stainless steels and a cost effective alternative to more expensive nickel-base alloys where excellent formability, weldability, strength and corrosion resistance are essential.

|
|
|
|
|