SS310/1.4845/UNS31000
Add Time: 2013-9-2 13:29:54 Source: ×÷Õß: µã»÷Êý:3214
SS310/1.4845/UNS31000
Stainless steel 310/310S is an austenitic heat resistant alloy with excellent resistance to oxidation under mildly cyclic conditions through 2000ºF. Its high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation and the retention of a larger fraction of room temperature strength than the common austenitic alloys like Type 304. Stainless 310 is often used at cryogenic temperatures, with excellent toughness to -450¡ãF, and low magnetic permeability.
 
Copyright©2006 Zhengbang Super Alloy Ltd. Right Reserved.
Tel: 86-(0)527-80686558 Fax: 86-(0)527-89881187 Email: admin@zbindustry.com admin@zbsuperalloy.com